![Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.](/rev13959/modules/../customized/tradenames/views/images/seo_en.png)
Material datasheets available free. Online registration at: www.materialdatacenter.com
Radiflam A - PA66 - RadiciGroup High Performance Polymers
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Radiflam A" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...e standard at a thickness of 0.75mm. The GWFI is fulfilled at 960°C. The tracking resistance of both materials has an optimum value of 600 volts (CTI A). Alongside Radici with its proven range of flame-retardant PA 6 and 66 polyamides (Radiflam A and S) and also polybutylene terephthalate (Radiflam B), Rhodia Engineering Plastics also supplies a series of attractive polyamides. Technyl Star S 60G1 V30 is an easy-flowing polyamide 6 with 30% glass fibres and no halogen or red phosphorus, which a...
Kunststoffe international, 2005-11-21, More Reliable Washing
...ments on fire behaviour. Reliable Positioning Indispensable When the so-called Aqua Stop System was developed for Bauknecht-Whirlpool washing machines (title photo, Fig.1) the Robert Klinger GmbH company opted for the flame-retardant polyamide 66, Radiflam A FR, from Italian producer Radici. In order to fulfil the end customer’s stringent demands in terms of reliability and safety, the Klinger company had to come up with a new design for the microswitch holder. The aims here included - increas...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.